Reliance Industries Reclair R35042

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Reclair R35042.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reclair R35042 is a medium density polyethylene grade designed for the rotomoulding process. It exhibits good toughness and environmental stress resistance.Information provided by Reliance Industries
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.0 MPa
2030 psi
ASTM D368
Elongation at Yield 260 %
260 %
Flexural Modulus 0.480 GPa
69.6 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256