Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Reliance Industries Reclair F18020 Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Reclair F18020 Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Butene comonomer based Linear Low Density Polyethylene cast film grade. Reclair F18020 has optimum levels of antioxidants, and polymer processing aids. Applications:cast films, air bubble films, and films for lamination. Information provided by Reliance Industries
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min

@Load 2.16 kg
2.0 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.5 MPa
1810 psi
ASTM D882
Film Tensile Strength at Yield, TD 12.0 MPa
1740 psi
ASTM D882
Film Elongation at Break, MD 700 %
700 %
ASTM D882
Film Elongation at Break, TD 800 %
800 %
ASTM D882
Elmendorf Tear Strength, MD 2.00 g/micron
50.8 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 7.30 g/micron
185 g/mil
ASTM D1922
Dart Drop 3.00 g/micron
76.2 g/mil
F<sub>50</sub>,38mm dart 66mm height; ASTM D1709
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ASTM D882
Film Tensile Strength at Break, TD 25.0 MPa
3630 psi
ASTM D882
Users viewing this material also viewed the following: