Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RedEye On Demand Polyphenylsulfone (PPSF), Rapid Prototyping Material

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer RedEye On Demand
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RedEye On Demand Polyphenylsulfone (PPSF), Rapid Prototyping Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyphenylsulfone (PPSF) is a durable high-end thermoplastic that can be used in the toughest applications. Parts built in PPSF can handle heat near 400°F (204°C), it resists petroleum products, acids, and bases, and its strength is superior to other rapid prototyping thermoplastics. PPSF parts are built with a layered manufacturing process utilizing Fused Deposition Modeling (FDM) technology. This technology can build parts with high-performance engineering materials ideal for functional prototypes and end-use parts.Applications: Based on its high-performance properties of heat and chemical resistance, PPSF is ideal for engine components, covers and enclosures subject to heat, industrial machinery components or any application where the part needs to be functionally tested in an environment of heat or chemicals. Parts build in PPSF are also used as masters for RTV molds and vacuum forming.In a rapid manufacturing application, Polyphenylsulfone can be used to create actual production parts in lieu of injection molding for short-run production. Rapid (or layered) manufacturing provides multiple benefits:High design iterations – while in production the design engineer has the freedom to modify geometry’s on the fly which cannot be done once committed to toolingBridge manufacturing – with rapid manufactured parts, production can begin while permanent tooling is on order Jigs and Fixtures to be used on manufacturing/production linesFor those manufacturers who practice lean manufacturing techniques or who maintain just-in-time inventories, RM can conserve cash flowAlpha and beta product releases – manufacturers can produce accurate, durable products even in the earliest stages of production
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 86
86
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
Type 1, 0.125; ASTM D638
Elongation at Yield 3.0 %
3.0 %
Tensile, Type 1, 0.125; ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
Type 1, .0125; ASTM D638
Flexural Strength 110 MPa
15900 psi
ASTM D790
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 0.5873 J/cm
1.100 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 31.0 µm/m-°C

@Temperature 20.0 °C
17.2 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
ASTM D648
Glass Transition Temp, Tg 230 °C
446 °F
DMA (SSYS)
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Constant 3.45

@Frequency 60 Hz
3.45

@Frequency 60 Hz
IEC 60250
Dielectric Strength 14.6 kV/mm
371 kV/in
IEC 60112
Descriptive Properties Value Comments
Color Tan
Environmental Res. to Windshield Washer Fluid, 50% Passed
24 hours @ 23°C
Passed
24 hours @ 100°C
Environmental Resistance to Antifreeze Passed
24 hours @ 23°C
Passed
24 hours @ 100°C
Environmental Resistance to Motor Oil 10W-40 Passed
24 hours @ 23°C
Passed
24 hours @ 100°C
Environmental Resistance to Power Steering Fluid Passed
24 hours @ 23°C
Passed
24 hours @ 100°C
Environmental Resistance to Transmission Fluid Passed
24 hours @ 23°C
Passed
24 hours @ 100°C
Environmental Resistance to Unleaded Gasoline Passed
24 hours @ 23°C
untested
24 hours @ 100°C
Users viewing this material also viewed the following: