RedEye On Demand PC/ABS for FDM Rapid Prototyping

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer RedEye On Demand
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RedEye On Demand PC/ABS for FDM Rapid Prototyping.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This thermoplastic polymer blend combines PC (Polycarbonate) and ABS (Acrylonitrile Butadiene Styrene) to produce an industrial material with a lot to offer. It combines the strength of PC with the flexibility of ABS. With excellent heat-resistance and mechanical properties, it is significantly stronger than ABS. PC/ABS parts are built with a layered manufacturing process utilizing Fused Deposition Modeling (FDM) technology, often used in rapid prototyping. Parts produced from this technology will maintain dimensional stability.ApplicationsPC/ABS is an affordable option where strength and rigidity are necessary in conjunction with toughness and temperature tolerance. It produces parts with good surface appeal. This blend is widely used in industries such as automotive, electronics, toys and telecommunications. Parts built from PC/ABS can also be used as masters for RTV molds and vacuum forming, vacuum metallization, electroplating, and parts that require snap fitsWhen used in FDM, this blend is ideal for the rapid production of prototypes, tooling and rapid manufacturing of production parts in lieu of injection molding. Rapid (or layered) manufacturing provides multiple benefits:High design iterations – while in production the design engineer has the freedom to modify geometry’s on the fly which cannot be done once you have committed to toolingBridge manufacturing – with rapid manufactured parts, production can begin while permanent tooling is on orderJigs and Fixtures to be used on manufacturing/production linesFor those manufacturers who practice lean manufacturing techniques or who maintain just-in-time inventories, RM can conserve cash flowAlpha and beta product releases – manufacturers can produce accurate, durable products even in the earliest stages of production
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
Tensile Strength, Yield 34.8 MPa
5050 psi
ASTM D638
Elongation at Break 4.3 %
4.3 %
ASTM D638
Tensile Modulus 1.827 GPa
265.0 ksi
ASTM D638
Flexural Yield Strength 50.0 MPa
7250 psi
ASTM D790
Flexural Modulus 1.863 GPa
270.2 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.26 J/cm
6.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
ASTM D648
Vicat Softening Point 112 °C
234 °F
ASTM D1525
Glass Transition Temp, Tg 125 °C
257 °F
DMA (SYSS)
Flammability, UL94 HB

@Thickness 0.850 mm
HB

@Thickness 0.0335 in
Electrical Properties Metric English Comments
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
IEC 60250
3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60112