Ravago Manufacturing Americas Hysun™ 693 ASA  (discontinued **)

Category Polymer , Thermoplastic , ASA Polymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hysun™ 693 ASA  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
0.125 in; ASTM D955
Melt Flow 4.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 84
84
ASTM D785
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
73°F, 0.125 in; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature -40.0 - 176 °C
61.0 µin/in-°F

@Temperature -40.0 - 349 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
Unannealed (0.250 in); ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Unannealed (0.250 in); ASTM D648