Ravago Manufacturing Americas Hysun™ 383 ASA  (discontinued **)

Category Polymer , Thermoplastic , ASA Polymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hysun™ 383 ASA  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 1.93 GPa
280 ksi
ASTM D638
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
73°F, 0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
Unannealed (0.250 in); ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Unannealed (0.250 in); ASTM D648
Vicat Softening Point 90.0 °C
194 °F
Rate A; ASTM D1525