Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1213HL BK Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Reinforced, Impact Grade
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1213HL BK Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Filler: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Processing Method: Injection Molding Color: BlackInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.00060 - 0.00090 cm/cm
0.00060 - 0.00090 in/in
ASTM D955 and ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength at Break 103 MPa
14900 psi
ISO 527-2
103 MPa
15000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 165 MPa
23900 psi
ISO 178
165 MPa
24000 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
4.48 GPa
650 ksi
ISO 178
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 2.94 kJ/m²
1.40 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
15.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
Unannealed; ASTM D648