Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylex® P1018FRVNHE Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylex® P1018FRVNHE Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate, 18 Melt Flow, Flame Retardant, Non HalogenatedInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm

@Thickness 3.17 mm
0.0050 - 0.0070 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0 - 5VA

@Thickness 3.00 mm
V-0 - 5VA

@Thickness 0.118 in
Copyright © lookpolymers.com All Rights Reserved