Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Echo® RPC10G BK Polypropylene Homopolymer

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Glass Fiber Filler
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Echo®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Echo® RPC10G BK Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Filler: Glass Fiber Reinforcement, 10% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
ASTM D792
Filler Content 10 %
10 %
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Modulus 2.96 GPa
429 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: