Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Raditer® BN100 Polybutylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Raditer® BN100 Polybutylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PBT General PurposeInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-1/2
Elongation at Break 35 %
35 %
ISO 527-1/2
Elongation at Yield 8.5 %
8.5 %
ISO 524-1/2
Tensile Modulus 2.75 GPa
399 ksi
ISO 527-1/2
Flexural Strength 80.0 MPa
11600 psi
ISO 178
Flexural Modulus 2.20 GPa
319 ksi
ISO 178
Charpy Impact, Notched 0.420 J/cm²
2.00 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75/2Af
Vicat Softening Point 180 °C
356 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Copyright © lookpolymers.com All Rights Reserved