Radici Radilon® WIT 30/28 Nylon 66-GF30

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® WIT 30/28 Nylon 66-GF30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive cooling liquid resistant PA66-GF30 grade designed to be processed by WIT technology.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Water Absorption 1.7 %
1.7 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Tensile Modulus 8.40 GPa
1220 ksi
ISO 527
Flexural Modulus 7.20 GPa
1040 ksi
ISO 178
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in