Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® SRV300 (dry) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber/Solid Lube Filled
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® SRV300 (dry) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass-fiber reinforcedInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 170 MPa
24700 psi
ISO 527-1/2
Elongation at Break 3.8 %
3.8 %
ISO 527-1/2
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527-1/2
Flexural Strength 250 MPa
36300 psi
ISO 178
Flexural Modulus 7.95 GPa
1150 ksi
ISO 178
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75/2Af
Vicat Softening Point 210 °C
410 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Users viewing this material also viewed the following: