Material Notes:
General PurposeInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527-1/2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/2
Elongation at Yield 4.1 %
4.1 %
ISO 524-1/2
Tensile Modulus 3.05 GPa
442 ksi
ISO 527-1/2
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 2.35 GPa
341 ksi
ISO 178
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 1135 7-1-3
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75/2Af
Vicat Softening Point 190 °C
374 °F
ISO 306
Flammability, UL94 V-2

@Thickness 0.800 mm
V-2

@Thickness 0.0315 in