Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® S USX200 (dry) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® S USX200 (dry) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Water Absorption 7.6 %
7.6 %
Moisture Absorption at Equilibrium 2.0 %
2.0 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 4.4 %
4.4 %
Tensile Modulus 1.65 GPa
239 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 1.60 J/cm²

@Temperature -30.0 °C
7.61 ft-lb/in²

@Temperature -22.0 °F
8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Vicat Softening Point 150 °C

@Load 5.10 kg
302 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
Users viewing this material also viewed the following: