Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® S RV300R (cond.) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® S RV300R (cond.) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
(Dry)
Water Absorption 6.7 %
6.7 %
initially dry
Moisture Absorption at Equilibrium 2.0 %
2.0 %
initially dry
Viscosity Measurement 140
140
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
Elongation at Break 4.3 %
4.3 %
Tensile Modulus 7.20 GPa
1040 ksi
Charpy Impact Unnotched 8.50 J/cm²

@Temperature -30.0 °C
40.4 ft-lb/in²

@Temperature -22.0 °F
9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved