Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
Water Absorption 5.8 %
5.8 %
Moisture Absorption at Equilibrium 1.9 %
1.9 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
Elongation at Break 8.5 %
8.5 %
Tensile Modulus 6.25 GPa
906 ksi
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.280 J/cm²

@Temperature -30.0 °C
1.33 ft-lb/in²

@Temperature -22.0 °F
0.420 J/cm²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 0.46 MPa (66 psi) 195 °C
383 °F
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm