Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® S CP400 (cond.) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® S CP400 (cond.) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
(Dry)
Water Absorption 5.8 %
5.8 %
initially dry
Moisture Absorption at Equilibrium 1.9 %
1.9 %
initially dry
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
Elongation at Break 30 %
30 %
Nominal
Elongation at Yield 17 %
17 %
Tensile Modulus 2.60 GPa
377 ksi
Charpy Impact Unnotched 7.00 J/cm²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V