Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Water Absorption 0.40 %
0.40 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Elongation at Break 1.5 %
1.5 %
ASTM D638
Modulus of Elasticity 14.0 GPa
2030 ksi
ASTM D638
Flexural Yield Strength 180 MPa
26100 psi
ASTM D570
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
UL94