Material Notes:
Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 17 %
17 %
Tensile Modulus 0.750 GPa
109 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
Charpy Impact, Notched 13.0 J/cm²

@Temperature 23.0 °C
61.9 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V