Radici Radilon® CARV300 L (dry) Copolyamide 66/6

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/Nylon 6 Blend, Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® CARV300 L (dry) Copolyamide 66/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass-fiber reinforcedInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 165 MPa
23900 psi
ISO 527-1/2
Elongation at Break 3.3 %
3.3 %
ISO 527-1/2
Tensile Modulus 10.3 GPa
1490 ksi
ISO 527-1/2
Flexural Strength 240 MPa
34800 psi
ISO 178
Flexural Modulus 8.15 GPa
1180 ksi
ISO 178
Charpy Impact Unnotched 6.80 J/cm²
32.4 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ISO 75/2Af
Vicat Softening Point 225 °C
437 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in