Material Notes:
General purposeInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527-1/2
Elongation at Break 35 %
35 %
ISO 527-1/2
Elongation at Yield 3.9 %
3.9 %
ISO 524-1/2
Tensile Modulus 3.00 GPa
435 ksi
ISO 527-1/2
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75/2Af
Vicat Softening Point 210 °C
410 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in