Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® AUSX200 (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® AUSX200 (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Very high impact strengthInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527-1/2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/2
Elongation at Yield 7.0 %
7.0 %
ISO 524-1/2
Tensile Modulus 1.85 GPa
268 ksi
ISO 527-1/2
Flexural Strength 55.0 MPa
7980 psi
ISO 178
Flexural Modulus 1.35 GPa
196 ksi
ISO 178
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75/2Af
Vicat Softening Point 170 °C
338 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Users viewing this material also viewed the following: