Radici Radilon® A RCF3505 (cond.) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A RCF3505 (cond.) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
(Dry)
Water Absorption 5.3 %
5.3 %
initially dry
Moisture Absorption at Equilibrium 1.2 %
1.2 %
initially dry
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa
23200 psi
Elongation at Break 1.9 %
1.9 %
Tensile Modulus 18.9 GPa
2740 ksi
Charpy Impact Unnotched 4.50 J/cm²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.640 J/cm²

@Temperature -30.0 °C
3.05 ft-lb/in²

@Temperature -22.0 °F
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 10 ohm-cm
10 ohm-cm
Surface Resistance 10 ohm
10 ohm
Comparative Tracking Index 150 V
150 V