Radici Radilon® A HSX (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A HSX (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
Water Absorption 7.6 %
7.6 %
Moisture Absorption at Equilibrium 2.0 %
2.0 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
Elongation at Break 35 %
35 %
Nominal
Elongation at Yield 4.5 %
4.5 %
Tensile Modulus 2.75 GPa
399 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
1.60 J/cm²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Vicat Softening Point 225 °C

@Load 5.10 kg
437 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm