Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
Water Absorption 5.7 %
5.7 %
Moisture Absorption at Equilibrium 1.8 %
1.8 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
Elongation at Break 7.2 %
7.2 %
Tensile Modulus 5.85 GPa
848 ksi
Charpy Impact Unnotched 5.50 J/cm²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
0.340 J/cm²

@Temperature 23.0 °C
1.62 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Vicat Softening Point 220 °C

@Load 5.10 kg
428 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm