Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Water Absorption 8.4 %
8.4 %
Moisture Absorption at Equilibrium 2.1 %
2.1 %
Viscosity Measurement 240
240
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength, Yield 95.0 MPa
13800 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 4.0 %
4.0 %
Tensile Modulus 3.25 GPa
471 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 0.46 MPa (66 psi) 195 °C
383 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Vicat Softening Point 240 °C

@Load 5.10 kg
464 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm