Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radiflam® B RV 300 AE Polybutylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® B RV 300 AE Polybutylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Raditer® B RV 300AE is a glass fiber reinforced, self-extinguishing UL-94 V-0 (with halogen) thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properties with very good dimensional stability.Suggestions for application: Technical items with good electrical properties, coloring and stiffness.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.57 g/cc
1.57 g/cc
ISO 1183
Moisture Absorption at Equilibrium 0.15 %
0.15 %
ISO 62
Mechanical Properties Metric English Comments
Elongation at Break 110 %
110 %
ISO 527-2/1A
Tensile Modulus 9.00 GPa
1310 ksi
ISO 527-2/1A
Flexural Strength 160 MPa
23200 psi
ISO 178/1A
Flexural Modulus 7.20 GPa
1040 ksi
ISO 178/1A
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179 eU
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ISO 11357-1-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-2/Af
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-2/Af
Vicat Softening Point 200 °C

@Load 5.10 kg
392 °F

@Load 11.2 lb
50°C/h; ISO 306/B50
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
CEI 695-2-1/2
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved