Radici Radiflam® ARV300 AE (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® ARV300 AE (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA66 Self-extinguishing glass-fiber reinforced with halogensInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.61 g/cc
1.61 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 155 MPa
22500 psi
ISO 527-1/2
Elongation at Break 2.1 %
2.1 %
ISO 527-1/2
Tensile Modulus 12.35 GPa
1791 ksi
ISO 527-1/2
Flexural Strength 240 MPa
34800 psi
ISO 178
Flexural Modulus 10.8 GPa
1570 ksi
ISO 178
Charpy Impact Unnotched 5.60 J/cm²
26.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.950 J/cm²
4.52 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ISO 75/2Af
Vicat Softening Point 240 °C
464 °F
ISO 306
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in