Radici Radiflam® AFR (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® AFR (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA66 Self-extinguishing without halogens or phosphorousInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527-1/2
Elongation at Break 3.5 %
3.5 %
ISO 527-1/2
Tensile Modulus 3.50 GPa
508 ksi
ISO 527-1/2
Flexural Strength 110 MPa
16000 psi
ISO 178
Flexural Modulus 3.00 GPa
435 ksi
ISO 178
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75/2Af
Vicat Softening Point 220 °C
428 °F
ISO 306
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in