Material Notes:
PA66 flame retardant injection molding grade. Halogens and phosphorus free. Natural color. Suitable for monofilament extrusion.Information provided by Radici group.
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: