Radici Heraflex® P 40D 21 I HF Modified Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Radici Group Plastics
Trade Name Heraflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Heraflex® P 40D 21 I HF Modified Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shore hardness: 40D (3s)Shiny surface, very flexible even at very low T°C (to -30°C), good resistance to weather conditions, very light and recyclableApplication examples: low price, boots internal parts, winter footwear, ski boots, sports shoesInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 40

@Time 3.00 sec
40

@Time 0.000833 hour
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -30.0 °C
-22.0 °F