Radici Heraflex® E 5620 TPC-ET Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Radici Group Plastics
Trade Name Heraflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Heraflex® E 5620 TPC-ET Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPC-ET Thermoplastic Elastomer. Medium Modulus, Nominal Shore D/15s 50. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Water Absorption 0.29 %

@Time 86400 sec
0.29 %

@Time 24.0 hour
MI / 08
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
Instantaneous; ISO 868
50

@Time 15.0 sec
50

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 43.0 MPa
6240 psi
ISO 527-1/2
Elongation at Break 688 %
688 %
ISO 527 1/2
Flexural Modulus 0.221 GPa
32.1 ksi
ISO 178/1A
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 174 kN/m
993 pli
ASTM D1004
Abrasion 15
15
mm<sup>3</sup>; DIN 53516
Thermal Properties Metric English Comments
Melting Point 199 °C
390 °F
Vicat Softening Point 177 °C

@Load 5.10 kg
351 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V