Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Radici Group Plastics
Trade Name Heraflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPC-ET Thermoplastic Elastomer. Lowest Modulus, Nominal Shore D/15s 35. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Water Absorption 0.73 %

@Time 86400 sec
0.73 %

@Time 24.0 hour
MI / 08
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 230 °C
34 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 39
39
Instantaneous; ISO 868
35

@Time 15.0 sec
35

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 26.0 MPa
3770 psi
ISO 527-1/2
Elongation at Break 968 %
968 %
ISO 527 1/2
Flexural Modulus 0.0590 GPa
8.56 ksi
ISO 178/1A
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 113 kN/m
645 pli
ASTM D1004
Abrasion 26
26
mm<sup>3</sup>; DIN 53516
Thermal Properties Metric English Comments
Melting Point 180 °C
356 °F
Vicat Softening Point 128 °C

@Load 5.10 kg
262 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V