Radici Heraflex® A 55 I RKT TPS-SEBS Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Radici Group Plastics
Trade Name Heraflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Heraflex® A 55 I RKT TPS-SEBS Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shore hardness: 55A (3s)Transparent, scratch resistant and high heat resistanceApplication examples: soft touch, housewares, tool handles, toys, PP overmoldingInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified