Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Heraflex® A 55 11 I HW TPS-SEBS Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Radici Group Plastics
Trade Name Heraflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Heraflex® A 55 11 I HW TPS-SEBS Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shore hardness: 55A (3s)Translucent, scratch resistant and high heat resistanceApplication examples: hooves, gaskets, sanitary goodsInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Copyright © lookpolymers.com All Rights Reserved