Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D 792
Filler Content 10 %
10 %
Primary Additive
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm

@Thickness 3.17 mm
0.0020 - 0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ASTM D 638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D 638
Tensile Modulus 6.89 GPa
1000 ksi
ASTM D 638
Flexural Strength 179 MPa
26000 psi
ASTM D 790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D 790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Processing Properties Metric English Comments
Melt Temperature 332 - 371 °C
630 - 700 °F
Mold Temperature 93.3 - 149 °C
200 - 300 °F
Drying Temperature 135 °C
275 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi