RTP Company RTP 900 TFE 20  Polysulfone (PSU) PTFE 20%  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU) , Polysulfone with PTFE/Silicone Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 900 TFE 20  Polysulfone (PSU) PTFE 20%  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE 20%Comments:PTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
ASTM D955
0.0080 cm/cm

@Thickness 6.35 mm
0.0080 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 5.0 - 6.0 %
5.0 - 6.0 %
ASTM D638
Modulus of Elasticity 2.41 GPa
350 ksi
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Compressive Yield Strength 62.1 MPa
9000 psi
ASTM D695
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.259 W/m-K
1.80 BTU-in/hr-ft²-°F
Through-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 16.9 kV/mm
430 kV/in
S/T; ASTM D149
Dissipation Factor 0.0040

@Frequency 1e+6 Hz
0.0040

@Frequency 1e+6 Hz
Dry; ASTM D150
Processing Properties Metric English Comments
Processing Temperature 321 - 360 °C
610 - 680 °F
Mold Temperature 93.3 - 149 °C
200 - 300 °F
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Descriptive Properties Value Comments
Color Natural/Black