Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D 792
Additive Loading 10 %
10 %
Primary Additive
Linear Mold Shrinkage 0.0070 - 0.012 cm/cm

@Thickness 3.17 mm
0.0070 - 0.012 in/in

@Thickness 0.125 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.8 MPa
11000 psi
ASTM D 638
Elongation at Break 3.5 - 6.0 %
3.5 - 6.0 %
ASTM D 638
Tensile Modulus 4.48 GPa
650 ksi
ASTM D 638
Flexural Strength 117 MPa
17000 psi
ASTM D 790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D 790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 182 - 218 °C
360 - 425 °F
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Drying Temperature 121 °C

@Time 7200 sec
250 °F

@Time 2.00 hour
Moisture Content 0.15 %
0.15 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi