Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D 792
Filler Content 5 %
5 %
Primary Additive
Linear Mold Shrinkage 0.013 - 0.018 cm/cm

@Thickness 3.17 mm
0.013 - 0.018 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D 638
Elongation at Break 7.0 - 10 %
7.0 - 10 %
ASTM D 638
Tensile Modulus 3.45 GPa
500 ksi
ASTM D 638
Flexural Strength 86.2 MPa
12500 psi
ASTM D 790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D 790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 6.67 J/cm

@Thickness 3.17 mm
12.5 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 182 - 218 °C
360 - 425 °F
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Drying Temperature 121 °C
250 °F
Dry Time 2 hour
2 hour
Moisture Content 0.15 %
0.15 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi