RTP Company RTP 800 TFE 13 SI 2 Acetal (POM), PTFE & Silicone Lubricated

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, PTFE Filled
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 800 TFE 13 SI 2 Acetal (POM), PTFE & Silicone Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D 792
Filler Content 13 %
13 %
Primary Additive
Linear Mold Shrinkage 0.020 cm/cm

@Thickness 3.17 mm
0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.4 MPa
6000 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D 638
Flexural Strength 62.1 MPa
9000 psi
ASTM D 790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D 790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D 648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 182 - 218 °C
360 - 425 °F
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Drying Temperature 121 °C
250 °F
Dry Time 2 hour
2 hour
Moisture Content 0.15 %
0.15 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi