Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D 792
Additive Loading 1.0 %
1.0 %
Primary Additive
Linear Mold Shrinkage 0.015 - 0.025 cm/cm

@Thickness 3.20 mm
0.015 - 0.025 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.6 MPa
8500 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D 638
Flexural Strength 82.7 MPa
12000 psi
ASTM D 790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D 790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.20 mm
1.30 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB

@Thickness 3.20 mm
NB

@Thickness 0.126 in
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
240 °F
ASTM D 648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 182 - 218 °C
360 - 425 °F
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Drying Temperature 121 °C

@Time 7200 sec
250 °F

@Time 2.00 hour
Moisture Content 0.15 %
0.15 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi