Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 799 X 50492 L Low Density Polyethylene (LDPE), Electrically Conductive

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 799 X 50492 L Low Density Polyethylene (LDPE), Electrically Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D 792
Linear Mold Shrinkage 0.018 - 0.028 cm/cm

@Thickness 3.17 mm
0.018 - 0.028 in/in

@Thickness 0.125 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 0.276 GPa
40.0 ksi
ASTM D 638
Flexural Strength 10.0 MPa
1450 psi
ASTM D 790
Flexural Modulus 0.276 GPa
40.0 ksi
ASTM D 790
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm
9.00 ft-lb/in

@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
Electrical Properties Metric English Comments
Volume Resistivity <= 1e+05
<= 1e+05
ASTM D 257
Surface Resistance <= 1.00e+7 ohm
<= 1.00e+7 ohm
ESD STM11.11
Surface Resistivity per Square <= 1.00e+8 ohm
<= 1.00e+8 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 193 - 232 °C
380 - 450 °F
Mold Temperature 21.1 - 65.6 °C
70.0 - 150 °F
Drying Temperature 79.4 °C

@Time 7200 sec
175 °F

@Time 2.00 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi