RTP Company RTP 506 HB Styrene Acrylonitrile (SAN), Glass Fiber - UL94 HB

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 506 HB Styrene Acrylonitrile (SAN), Glass Fiber - UL94 HB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The RTP 500 series of glass fiber reinforced SAN materials offers improved strengths over the base resin. This series has an excellent balance of properties and is one of the most cost effective RTP Company series.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D 792
Filler Content 35 %
35 %
Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.17 mm
0.00050 - 0.0015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D 785
Tensile Strength at Break 121 MPa
17500 psi
ASTM D 638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D 638
Tensile Modulus 12.1 GPa
1750 ksi
ASTM D 638
Flexural Strength 165 MPa
24000 psi
ASTM D 790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D 790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 2.40 J/cm

@Thickness 3.17 mm
4.50 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 238 - 279 °C
460 - 535 °F
Mold Temperature 51.7 - 82.2 °C
125 - 180 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 2 hour
2 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi