Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 4799 X 121826 C Biobased Polyester Permanently Anti-static - ESD Protection - 29% Bio-Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polytrimethylene Terephthalate (PTT)
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 4799 X 121826 C Biobased Polyester Permanently Anti-static - ESD Protection - 29% Bio-Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D 792
Linear Mold Shrinkage 0.020 cm/cm

@Thickness 3.20 mm
0.020 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.4 MPa
6000 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D 638
Flexural Strength 68.9 MPa
10000 psi
ASTM D 790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D 790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.20 mm
1.20 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB

@Thickness 3.20 mm
NB

@Thickness 0.126 in
ASTM D 4812
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 - 1.00e+10 ohm-cm
1.00e+9 - 1.00e+10 ohm-cm
ASTM D 257
Surface Resistivity per Square 1.00e+10 - 1.00e+11 ohm
1.00e+10 - 1.00e+11 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 204 - 238 °C
400 - 460 °F
Mold Temperature 37.8 - 121 °C
100 - 250 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content 0.030 %
0.030 %
Dew Point -28.9 °C
-20.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi