RTP Company RTP 4500 TFE 10 Aliphatic Polyketone, PTFE 10%  (discontinued **)

Category Polymer , Thermoplastic , Polyketone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 4500 TFE 10 Aliphatic Polyketone, PTFE 10%  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties and average values of injection molded specimens; data provided by RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Linear Mold Shrinkage 0.030 cm/cm

@Thickness 3.17 mm
0.030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Tensile Modulus 1.70 GPa
247 ksi
ASTM D638
Flexural Yield Strength 50.0 MPa
7250 psi
ASTM D790
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 3.17 mm
2.06 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 14.4 J/cm

@Thickness 3.17 mm
27.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
ASTM D648