Material Notes:
Properties are based on annealled specimens.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D 792
Filler Content 20 %
20 %
Primary Additive
Linear Mold Shrinkage 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa
20000 psi
ASTM D 638
Elongation at Break 3.5 %
3.5 %
ASTM D 638
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D 638
Flexural Strength 214 MPa
31000 psi
ASTM D 790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D 790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm
1.90 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 8.81 J/cm

@Thickness 3.17 mm
16.5 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 288 °C
550 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Processing Properties Metric English Comments
Melt Temperature 399 - 416 °C
750 - 780 °F
Mold Temperature 177 - 232 °C
350 - 450 °F
Drying Temperature 204 °C
400 °F
Dry Time 6 hour
6 hour
Moisture Content 0.010 %
0.010 %
Dew Point -40.0 °C
-40.0 °F
Injection Pressure 138 - 193 MPa
20000 - 28000 psi