RTP Company RTP 4099X67316A Polyphthalamide, GF, Stainless Steel Fiber, EMI  (discontinued **)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Stainless Fiber Filled/EMI
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 4099X67316A Polyphthalamide, GF, Stainless Steel Fiber, EMI  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data is for injection molded specimens and was provided by the manufacturer, RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs @ 23°C; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 6.40 mm
0.0040 in/in

@Thickness 0.252 in
ASTM D955
0.0040 cm/cm

@Thickness 3.20 mm
0.0040 in/in

@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 159 MPa
23100 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Tensile Modulus 9.00 GPa
1310 ksi
ASTM D638
Flexural Yield Strength 262 MPa
38000 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm

@Thickness 3.20 mm
1.12 ft-lb/in

@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 5.90 J/cm

@Thickness 3.20 mm
11.1 ft-lb/in

@Thickness 0.126 in
ASTM D256
K (wear) Factor 10100 x 10-8 mm³/N-M
5000 x 10-10 in³-min/ft-lb-hr
at 50 fpm, 2000 PV against C1018 Steel HRC 15-25, 14-17 microsmoothness; ASTM D 3702
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 266 °C
511 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB; UL94. Values per RTP Company Testing.
Electrical Properties Metric English Comments
Electrical Resistivity 16.0 ohm-cm
16.0 ohm-cm
ASTM D257