Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 4099 X 128640 Polyphthalamide (PPA), Thermally Conductive - Electrically Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Preliminary Data Sheet
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.7 MPa
12000 psi
ASTM D 638
Elongation at Break <= 1.0 %
<= 1.0 %
ASTM D 638
Tensile Modulus 13.8 GPa
2000 ksi
ASTM D 638
Flexural Strength 103 MPa
15000 psi
ASTM D 790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D 790
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm
0.500 ft-lb/in

@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D 4812
Thermal Properties Metric English Comments
Thermal Conductivity 1.00 W/m-K
6.94 BTU-in/hr-ft²-°F
Through-plane; ASTM E 1530
5.003 W/m-K
34.72 BTU-in/hr-ft²-°F
In-plane; ASTM E 1461-92
Electrical Properties Metric English Comments
Volume Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
ASTM D 257
Surface Resistance <= 1e+05
<= 1e+05
ESD STM11.11
Surface Resistivity per Square <= 1.00e+6 ohm
<= 1.00e+6 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 302 - 329 °C
575 - 625 °F
Mold Temperature 135 - 163 °C
275 - 325 °F
Drying Temperature 107 °C

@Time 14400 - 21600 sec
225 °F

@Time 4.00 - 6.00 hour
Moisture Content 0.050 %
0.050 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Copyright © lookpolymers.com All Rights Reserved