Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 4099 X 112302 Polyphthalamide (PPA), Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - Impact Modified

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Stainless Fiber Filled/EMI
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 4099 X 112302 Polyphthalamide (PPA), Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 76.5 MPa
11100 psi
ASTM D 638
Elongation at Break 6.0 %
6.0 %
ASTM D 638
Tensile Modulus 2.90 GPa
420 ksi
ASTM D 638
Flexural Strength 100 MPa
14500 psi
ASTM D 790
Flexural Modulus 2.90 GPa
420 ksi
ASTM D 790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D 648
Electrical Properties Metric English Comments
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ASTM D 257
Surface Resistance <= 1.00e+7 ohm
<= 1.00e+7 ohm
ESD STM11.11
Surface Resistivity per Square <= 1.00e+8 ohm
<= 1.00e+8 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
MIL-PRF-81705D, 5kV to 50 V, 12% RH|^|^; FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 313 - 329 °C
595 - 625 °F
Mold Temperature 135 - 163 °C
275 - 325 °F
Drying Temperature 107 °C

@Time 21600 sec
225 °F

@Time 6.00 hour
Moisture Content 0.040 %
0.040 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi