Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 4005A SI 2  Polyphthalamide - Hot Water Mold (PPA) Glass Fiber 30% - Silicone 2% &

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 4005A SI 2  Polyphthalamide - Hot Water Mold (PPA) Glass Fiber 30% - Silicone 2% &.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 30% - Silicone 2%Comments:Glass FiberSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 125
125
ASTM D785
Tensile Strength, Ultimate 169 MPa
24500 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Modulus of Elasticity 11.0 GPa
1600 ksi
ASTM D638
Flexural Yield Strength 262 MPa
38000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.86 J/cm

@Thickness 3.17 mm
9.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 277 °C
530 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 316 - 338 °C
600 - 640 °F
Mold Temperature 65.6 - 163 °C
150 - 325 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi